FORD C-MAX ( 26/09/2016 – 10/10/2016) DEFECT: A small batch of alloy wheels may have a casting defect that may initiate a fatigue crack and result in wheel failure.
Remedy
Check wheels on affected vehicles for a specific batch code. Replace those wheels which have the identified batch code.
| Recall Launch Date | 19/03/2018 |
| Recall No. | R/2018/011 |
| Models Affected | Focus C-Max |
| Manufacturer Ref | 17S38 |
| VIN Start | |
| VIN end | |
| Build Start | 26/09/2016 |
| Build end | 10/10/2016 |
| Vehicle numbers (UK) | 80 |
This notification is purely informative for the vehicle type you have selected. As these deficiencies often relate to specific components (engine type, bodywork, equipment), the recall may not apply to all vehicles of this type. For more detailed information on possible recalls for your vehicle, please get in touch with an authorised workshop (see below at "What the owner should do?").
What the owner should do?
Suppose you read about a recall that you think may affect your car. In that case, you should immediately contact a main dealer or workshop officially authorised to perform repairs on behalf of the manufacturer and ask for the details.
More Recalls
Recalls and Reliability
If you wish to know more about the eventual problems of a specific car (e.g. real mileage, potential traffic accident damages, odometer rollback, repairs, etc.), in that case, we suggest going to this page.
Currently 7104 Recalls